LOCATION:HOME >> NEWS >> Industry news
-
Industry news
A Fence Post Bends at the Ground Line, Not at the Top
A fence is quoted by the metre and paid for at the posts
A boundary fence looks continuous, but it is bought as posts with something stretched between them. A 200 metre run at three metre centres needs 67 line posts, and those posts carry most of the steel, most of the coating and all of the bending. Two numbers decide whether the fence stands in fifteen years: the moment at the ground line under a gust, and the rate the coating disappears below it.
Wind on a mesh panel is a small pressure until it is multiplied
A 30 metre per second gust, about 108 kilometres per hour, gives a velocity pressure of half of 1.25 times 30 squared, or 562 pascals. Mesh is not solid, so the force is reduced by its solidity, but by less than buyers assume. A welded mesh with a half-metre privacy strip, or a perforated Galvalume panel of the kind sold for fencing and screening, reaches about 25 per cent. That is 140 pascals on a three metre bay standing 2.4 metres high, 7.2 square metres, or 1,012 newtons.
The resultant sits near mid-height, 1.2 metres above grade, so the moment where the post leaves the soil is 1,012 times 1.2, or 1.22 kilonewton metres. Every line post in the run sees the same. A fence along the top of a slope or at the end of a building sees more, because the wind is compressed rather than deflected, and a corner post takes the load from two directions at once. Those fail first, and they are usually left out of the calculation.
What a 1.5 inch post does with 1.22 kilonewton metres
A 48.3 millimetre pipe at 3.68 millimetres wall, schedule 40 for one and a half inch bore, has a section modulus near 5,352 cubic millimetres. The A53 carbon steel pipe page gives Grade B a minimum yield of 35,000 psi, or 241 megapascals, so the section yields at 1.29 kilonewton metres. Demand 1.22 is 95 per cent utilisation before any gate or hedge. The post is not failing because the steel is poor, but because the section was chosen by bore rather than by bending.
One size up changes the picture. A 60.3 millimetre pipe at 3.91 millimetres wall reaches 2.21 kilonewton metres, 55 per cent; a 76.1 millimetre schedule 40 reaches 4.61. The square stainless steel pipe range runs from 10 by 10 mm up to 100 by 100 mm, and a 60 x 60 x 2 mm section in 201 has a modulus of 8,682 cubic millimetres. The 201 stainless steel page gives a transverse yield of 292 megapascals, so it reaches 2.53 kilonewton metres at 3.64 kilograms per metre against 5.44 for the pipe. A square puts its material further from the neutral axis, and 201 gives away nothing in strength.
The ground line is a different corrosion zone
Above ground a post dries between rain events. In the first 150 millimetres below the surface it does not: moisture stays, the oxygen supply changes with depth, and the band of alternating wet and dry is the most aggressive part of the fence. Fertiliser and road salt collect there. Zinc goes at roughly one to three micrometres a year, so coating mass decides life. The Z275 galvanized coil carries 275 grams per square metre, about 19 micrometres a face, or six to nineteen years; the 600 gram top of the SGCC galvanized sheet range is 42 micrometres a face and buys fourteen to forty-two. Coating applied after fabrication, on the hot-dipped galvanized coil route, is thicker still and covers the weld and the cut, which is why a fabricated post often outlasts a pre-coated one of the same nominal mass.
Where the ground is worse than ordinary, coating mass will not answer. The galvanized ERW pipe comparison notes that aggressive soil calls for a plant-applied barrier such as fusion-bonded epoxy, polyethylene tape or a three-layer polyethylene system, all applied before the post is cut. The A653 structural coil page shows the same 40 to 600 gram range on sheet.
Concrete, drainage and the water inside the tube
A line post needs a collar, not a footing. A hole 250 to 300 millimetres across and 600 to 700 deep, backfilled in compacted lifts, gives passive resistance in ordinary ground; the collar does not carry the fence, it stops the post rotating. The top should sit 100 millimetres below grade, sloped away from the steel.
The inside of the tube matters as much. An uncapped post fills with condensation and rain; a capped post that was not drained holds it until frost splits the weld at the base. Cap the top, drill a drain hole above the collar, and coat any mill-cut end with zinc-rich paint before it is buried.
The gate post carries something the line post does not
A gate leaf 1.8 metres wide and 1.5 metres high at 60 per cent solidity presents 1.62 square metres and takes about 910 newtons at 562 pascals. Near mid-leaf that is another 0.8 kilonewton metre on the hinge post, on top of the line load, and the eccentric weight of a leaf hung 50 millimetres off axis doubles it. The hinge post is the one post to size separately, usually at 88.9 millimetres. The latch post only has to hold the leaf closed, but if it shares concrete with the hinge post, movement at the hinge becomes a gate that will not latch.
Infill, fasteners and the cut end
The infill fixes the solidity the post was sized for, so it belongs on the drawing. A panel with 40 per cent open area is not a 40 per cent reduction against solid sheet, because frame and margins are solid, and a solid bottom strip can push effective solidity above plain mesh. Where the bottom half is sheet, the galvanized corrugated steel plate range covers thicknesses from 0.19 mm to 2 mm and widths up to 2,500 mm. Grade 201 suits inland; 316L stainless steel is the grade within sight of salt water, with 304 and 304L coil between the two.
Fasteners undo good posts. A stainless screw into a galvanized post makes zinc the anode, and the zinc area around the screw is small against the stainless head, so it goes quickly. Zinc-flake screws or a nylon washer keep the joint alive.
What to put on the order
The order should read: section and wall thickness, not nominal bore; 600 grams per square metre for the buried metre, or a plant-applied barrier; collar size; a separate gate post; infill solidity; fastener type. The Q235 plate for base plates is a minor line, but galvanize it after drilling. Ask for the coating mass on the mill certificate rather than the coating name, because Z275 on a 6 mm plate and Z275 on a 0.5 mm sheet are the same grams and very different years of life. A magnetic thickness gauge settles the argument in a minute.