A Pipe Span Is Set by What Is Inside It
Six metres of 168 mm tube
A 304 stainless line runs on a rack at 168.3 mm outside diameter and 3 mm wall, with supports 6 m apart. The drawing is usually checked for pressure and left there. Nobody asks what gravity does to the span, because a steel pipe looks stiff until it is filled. The same tube empty weighs 12.3 kg for every metre of run; full of water it weighs 33.0 kg. That difference, not the pressure rating, is what fixes how far apart the hangers can go.
What a metre of run actually weighs
The steel annulus is pi over four times 168.3 squared minus 162.3 squared, about 1,558 square millimetres, or 12.3 kg per metre at 7,900 kg per cubic metre. The bore is pi over four times 162.3 squared, 0.0207 square metres, so water adds 20.7 kg per metre. Fifty millimetres of insulation and a thin aluminium jacket add another 4 kg. A round tube programme running 8 to 680 mm outside diameter at 0.5 to 75 mm wall covers this size many times over; the 304L pipe listing covers outside diameters from 3 mm up to 2,200 mm and walls of 0.08 to 170 mm.
The section, the moment and the sag
Second moment of area is pi over 64 times 168.3 to the fourth minus 162.3 to the fourth, 5.32 by 10 to the 6 mm4, and the section modulus is that over half the diameter, 63,200 cubic millimetres. At 323.7 N per metre over 6 m a simply supported beam carries a mid-span moment of wL squared over 8, about 1,457 N.m, giving 23 MPa of bending stress. Mid-span sag is 5 w L to the fourth over 384 EI. With E near 193 GPa at room temperature, and the 310S sheet listing 200 GPa in tension, that is 5.3 mm. The serviceability limit of span over 360 allows 16.7 mm.
Stress never gets a vote here
Push the span out until bending stress reaches yield. At the 205 MPa yield floor quoted for 310S the allowable moment is 12,965 N.m, which puts the support spacing at 17.9 m. Even using 60 per cent of that leaves 13.9 m. The 201 sheet gives 197 GPa and a compressive yield of 365 MPa, which moves stiffness hardly at all and strength a long way. The sag limit, at 8.8 m, arrives first by a wide margin. Moving to a higher-strength grade buys nothing on a rack: E sits near 200 GPa for every austenitic grade in the catalogue.
Solve the other way round
Set sag equal to L over 360 and the span comes out of L cubed equals 384 EI over 1,800 w. For the full line that is 3.94 by 10 to the 8 over 5.83 by 10 to the 5, a cube root of 8.78 m. Empty, the same arithmetic gives 12.19 m. Filling the pipe shortens its permitted span by 28 per cent. A rack laid out for an empty line during erection, or for a gas line that later gets a liquid duty, is wrong by three and a half metres. The A106 seamless pressure pipe and the API 5L range at 4 to 1,219 mm and 1 to 60 mm wall are sized by pressure on most enquiries, and their support spacing is left to the field.
Why a bigger pipe does not span proportionally
For thin wall, I goes roughly as D cubed times t, steel weight as D times t, and the weight of the contents as D squared. With only self weight, allowed span goes as D to the two-thirds. With the bore full, w is dominated by D squared, and span goes as the cube root of D times t. Three sizes at a common wall: a 60.3 mm tube spans 5.2 m, the 168.3 mm line 8.8 m, and a 323.9 mm line with a 4 mm wall 12.5 m. Diameter grows 5.4 times while allowed span grows 2.4 times. The large-diameter range up to 2,500 mm and 150 mm wall is not five times farther between supports than a small line, and the A53 size range, which starts at half an inch and runs to 36 in NB, has to be read with that in mind.
Insulation and the test fill
Add 4 kg per metre of lagging to the 33.0 and the span drops from 8.78 to about 8.45 m, a 4 per cent trim that nobody puts on the drawing. Hydrostatic testing is worse. The line is filled, stationary and often at its heaviest before the permanent supports are all in place, and temporary stools are the first thing taken off the scaffold. A pipe that sags during the test keeps the sag: the cold bend is permanent, drains no longer fall to the low point, and the next shutdown finds water sitting in the belly. Permitted outside-diameter tolerances of 0.4 to 2.38 mm are tighter than that.
A valve is a point load, not a length of pipe
A flanged valve set on a 150 mm line is about 25 kg, 245 N, and at mid-span it adds P L cubed over 48 EI, roughly 1.1 mm, to the 5.3 mm of distributed sag. What the point load does is put a bending moment into the flange and a vibration node into the run, so the joint weeps rather than the pipe yielding. Valves, strainers and heavy tested pipe sections get their own support within a few hundred millimetres, whatever the span table says. The schedule ladder from SCH5 through SCH160 and XXS changes both weight and stiffness; a heavier schedule is not automatically a longer span once the contents are counted.
What the hanger touches
Supports are structures, not accessories. A carbon steel clamp on a wet 304 line is a galvanic couple and a crevice; a stainless or lined shoe costs little more. Square tube in sizes from 10 mm square up to 300 mm square makes trapeze frames, with Q345 plate for the base plates and galvanized plate for the brackets, all folded on a bending line and welded up. Punched slots rather than round holes let the line move with temperature. One fixed point, the rest sliding or guided, keeps thermal growth from turning a support into an anchor. For hot service the 310S pipe rated for continuous exposure near 2100 F is the metallurgy, but the spacing still comes from the sag sum.
Put the spans on the drawing
State outside diameter, wall and grade, then the density of what actually flows and the insulation build-up. Mark every valve, strainer and branch and give each a support. Name the fixed point and say which hangers slide. Order the welded versus seamless choice and the A53 schedule with the support steel, because the rack and the pipe arrive together. Tensile strength and a test pressure are what the certificate carries; the drawing has to show 8.8 m between hangers with the line full and 12.2 m empty. Get that wrong and the low point moves to mid-run.