LOCATION:HOME >> NEWS >> Industry news
-
Industry news
The Yield Number Starts at the Grain Boundary
Two plates carrying the same name
A Q235 plate and a second Q235 plate can leave one mill on the same morning and return tensile results fifty megapascals apart. No chemistry changed between them. What changed was the size of the ferrite grains at the moment rolling stopped. The Q235 listing calls the grade an indicator of yield strength and composition, and describes the slab being worked while new grains are still forming; both statements hold, and neither predicts what a coupon cut from the delivered piece will pull. Grain size appears on almost no enquiry form, yet it is the largest single term in the yield figure. Q345 and A36 are quoted the same way, as names with a floor attached. The grade survey is explicit that rolling refines the structure and leaves hot rolled stock with better ductility and toughness than cold rolled, which is a statement about grains even though it never uses the word. A buyer who reads only the designation has skipped the mechanism that sets the number.
The square root in the test result
The relationship is short: yield equals a baseline plus a coefficient divided by the square root of grain diameter. Take 70 MPa for the baseline and 0.6 MPa per square root metre for the coefficient, both typical published values for plain low carbon steel and used here as working figures rather than certificate data. At 50 micrometres the second term is 85 MPa and the sum is 155. At 20 micrometres it is 134 MPa and the sum is 204. At 10 micrometres, 190 and 260. At 5 micrometres, 268 and 338. Halving the diameter from 20 down to 10 adds 56 MPa on its own. The nominal 235 attached to Q235 sits roughly 31 MPa above the 20 micrometre result, and that remainder comes from carbon, manganese and pearlite, not from finer ferrite. Spreads like these are why Q195 stock, SPHC coil plate and 45 plate are bought on measured results as well as on name.
Why a thin gauge pulls higher
Reduction and cooling rate decide the grain, so thickness decides a good part of the strength. A thin strip takes more passes, finishes cooler and cools faster, and the grains have less time to grow before the coil is wound. Heavy plate finishes hotter and air-cools slowly through the same temperature window. This is the practical reason a single nominal grade is often quoted in thickness bands rather than as one flat figure. The DC01 sheet runs from 0.12 to 3.0 mm and is described as being rolled below the temperature at which new grains form, which is exactly the opposite condition from the 16Mn hot rolled coil programme. The distinction between the two routes is usually taught as a surface-finish difference; on the test machine it is a strength difference. ST12 sheet, cold rolled ST12 and A653 structural coil all sit on the thin side of that divide.
What an anneal does to the number
Cold reduction stretches the existing grains and packs dislocations into them, which raises strength while eating ductility. An anneal reverses the mechanism: fresh equiaxed grains nucleate and grow until the furnace is opened. Grain diameter after that step is set by time and temperature, and a line that runs a little hotter or holds a little longer hands the customer a softer coil with a lower yield. The DC01 process description and the Q345 hot rolled coil listing describe two ends of the same thermal story. A36 coil and 16Mn plate arrive from the hot line already recrystallised, with no separate furnace step behind them. Ordering a hardness band is not the same as ordering a grain size: the first is a reading taken after the fact, the second is the variable the mill actually controls.
The weld puts the coarse grain back
A weld undoes the refinement locally. In the heat affected zone the metal sits long enough at temperature for grains to coarsen, and the same square root now works against the designer. Let 20 micrometre base material grow to 50 in the coarse region and the calculated contribution falls from 134 to 85 MPa, a drop near 49 MPa, while toughness falls further still. Ferritic grades show it most plainly because there is no phase transformation to reset the structure: 430 is described as a non-hardenable straight chromium ferritic steel, and 409 is offered as a ferritic grade for exhaust work where weldability matters. 409 sheet and 410S sheet are bought into exactly those joints. A welded fabrication therefore needs the heat input and the joint location on the drawing, and the cut edge that will sit beside it needs the same attention.
Where alloying sits in the sum
Alloying adds terms to the baseline rather than replacing the grain term. The 317LMN data sheet names nitrogen as a strengthening agent and puts its yield above 317L, and the grade page gives the same account. Duplex structures get their strength partly from having two fine phases interleaved: 2507 is listed for exceptional strength, with LDX 2101 and 2205 on the leaner side of the same idea. The coil listings are worth reading carefully, because their finish tables use the words grain size for polishing abrasives: 201 coil, 202 strip and duplex coil all describe an HL finish produced with a suitable abrasive grit. That is a surface specification, not a metallurgical one, and confusing the two is an easy way to write a meaningless clause into an order.
What belongs on the enquiry
Ask for the measured yield on the certificate, the gauge it was taken from, and the delivery condition in which it was tested. Add a grain size determination against ASTM E112 when the part will be formed or welded, and accept heavy plate by thickness band rather than by a single melt result. The A36 construction guide and the grade survey both point to hot rolled stock for bending and load-bearing work, which is a ductility argument that finer grain supports. Frame schedules, welded assemblies and bent plate all consume that ductility. None of this makes the designation useless; it makes it a floor.
A number with a structure behind it
A mill that controls finishing temperature and total reduction controls the grain, and the grain controls most of what the tensile machine reports. The chemistry fills in the remaining thirty megapascals or so. When two certificates disagree, the useful questions are which gauge, which condition and which heat treatment, not which grade was printed at the top. Austenitic 304, the 1.4301 listing and Q345 plate are all ordered by name every day, and every one of them carries a microstructure that the name does not describe.